hygroscopic sulphates
#1
Posted 15 June 2009 - 08:23 AM
would it be acceptable to use the afore mentioned if it was bound with NC laquer and then primed, or would i be wasting time and chemicals ?
#2
Posted 15 June 2009 - 09:56 AM
Keep mannequins and watermelons away from fireworks..they always get hurt..
#3
Posted 15 June 2009 - 10:21 AM
#4
Posted 23 June 2009 - 06:05 AM
could someone please shed some light on the use of hygroscopic sulphates for strobe stars please, namely calcium sulphate and magnesium sulphate,
would it be acceptable to use the afore mentioned if it was bound with NC laquer and then primed, or would i be wasting time and chemicals ?
Hygroscopic compositions can be protected with waxes and various rubbers dissolved in solvents such as acetone. KNO3 and Sugar for instance is protected by paraffin oil or wax.
There is room for development. I imagine chlorowax could be used to protect copper sulfate. Though, I can't do such tests myself, so it only remains a suggested thought.
#5
Posted 24 June 2009 - 01:04 AM
NC is superior in this regard, which is why it is used in Ammonium perchlorate/Mg strobe compositions.
#6
Posted 24 June 2009 - 04:45 AM
The properties of the dry mix govern the properties of the product, if there is enough energy content then the water will be boiled off, or enter the reaction.
The properties of the stable comp govern the shelf life, once plaster has it's water or crystalisation then it absorbs no more from the air and the comp can stabilise, Lithium salts tend to go to a solution in their water accumulated by deliquescence and the comp can use this liquor to enable other reactions during standing, hence reducing the shelf life, including to the point of unusability.
Keep mannequins and watermelons away from fireworks..they always get hurt..
#7
Posted 25 June 2009 - 02:53 AM
Why would you mess with copper sulfate when blue and purple strobes are so easy with Potassium or barium sulfate?