Posted 29 June 2009 - 05:02 AM
Here is the synthesis I have. Strontium can probably be substituted for the barium.
Barium Peroxide
Preparation: Prepare a solution of 47g of barium chloride dihydrate in 250ml water. To this solution add 250ml 30% H2O2. Add 200ml 24% aqueous ammonia solution with stirring. Let the mixture stand until no more precipitate forms. Decant the clear portion, and replace the liquid with fresh water. Repeat the decanting 2-3 times. Filter on a Buchner funnel and wash with water. Dry in a porcelain cup at 50-70°C, occasionally spreading the powder with a spatula. After the product turns into a crumbly mass, increase the temperature to 75-80°C. Store the completely dried product in a tightly sealed bottle. Yield: 55-60g of the octahydrate. The product can be further dried to the hemihydrate at 130°C. The completely anhydrous peroxide can be obtained above 200°C, but a partial loss of oxygen will occur.