Posted 12 October 2010 - 09:31 PM
Yes, a thicker wall is a must if you're making it yourself.
Personally, I roll at least 5 layers of card for it not to burn away.
Nozzles should be made out of dry kitty litter.
I do not mean to patronise you, but was the nozzle hole at least 1/3 of the Inner Diameter of the fountain?
The plug is the last thing you make to fill the fountain up, so basically the plug you made at the start was meant to be the nozzle, you either use a drill bit or rather have a something which makes a hole in the plug when you ram it.
Also on kitty litter, do you attempt to powder it before you made the fountain? Or use it straight from the bag?
I tend to find that litter straight from the bag is the main cause of crumbling, mainly because the litter isn't incorporated together, and there's loads of air pockets which cause it to fall away, could be the cause of a weak nozzle.
I do wish I had some pyro buddies to help me out. That way I can actually go further than making small flares and fountains.