glitter strobe comp query

13 March 2011 - 07:44 PM

Experimenting with this Winokur formua (strobe pots instead of stars):

Winokur green Twinkler #1
49 Barium nitrate
18 Sulfur
11 MgAl, Granular, -60 mesh
9 MgAl, Granular, -200 mesh
6 Hexachloroethane
5 Dextrin
2 Potassium dichromate
0.5 Boric acid

. . . and wondering if it's assumed this is a water or water/alcohol binder--or is it kosher to bind with NC lacquer?

Also going way out on a limb with this one and subbing PVC for the Hexa- at a ratio of about half (3 or 4 parts instead of 6).